Hardened Alloy Steel
20CrMnTi / 8620 Case-Hardened Steel
Primary material for precision worm shafts. Case hardening provides a wear-resistant surface while maintaining a tough, ductile core for strength.
Material Data
- Composition
- Low-carbon alloy steel with Cr, Mn, Ti additives
- Hardness
- 58-62 HRC (surface), 28-32 HRC (core)
- Temperature Range
- -60°C to 250°C
- Price Index
- $$
- Standards
- DIN 17210, ASTM A29, JIS G4053, GB/T 3077
Strengths
- ✓Excellent surface hardness for wear resistance
- ✓Tough core resists impact and fatigue
- ✓Precision grindable to tight tolerances
- ✓Suitable for high-speed operation
- ✓Proven material for ground worm shafts
Limitations
- ✗Requires heat treatment (carburizing/nitriding)
- ✗Distortion risk during hardening
- ✗Must be ground after heat treatment
- ✗Higher machining cost than unhardened steel
- ✗Limited corrosion resistance without coating
Typical Applications
- ▸Precision worm shafts
- ▸Ground thread worm shafts
- ▸High-speed power transmission
- ▸Automotive steering worms
- ▸RV reducer worm shafts
Compatible Wheel Materials
This worm shaft material pairs best with the following wheel materials:
Applicable Standards
Hardened Alloy Steel — Frequently Asked Questions
What is case hardening and why is it used for worm shafts?
Case hardening (carburizing or carbonitriding) creates a hard, wear-resistant surface layer (58-64 HRC, 0.5-1.5mm deep) while keeping the core tough and ductile (28-32 HRC). This combination is ideal for worm shafts because the hard surface resists abrasive wear from the bronze wheel, while the tough core withstands bending and torsional loads without brittle fracture.
Which steel grades do you recommend for precision worm shafts?
For precision ground worm shafts: 16MnCr5 (DIN), 8620 (AISI), SCM420 (JIS), and 20CrMnTi (GB). For larger shafts where nitriding is preferred: 42CrMo4 or 4140. For automotive EPS applications: 16MnCr5 or SAE 8620 due to their excellent carburizing response and grindability.
How much distortion occurs during case hardening?
Carburizing and quenching typically causes 0.05-0.15% dimensional change. For precision worm shafts, we grind the thread profile after heat treatment to achieve final tolerances. Distortion is minimized by controlled atmosphere furnaces, press quenching for critical parts, and stress-relief tempering.
Can hardened steel worm shafts be re-ground if worn?
Yes, if wear is limited to the surface finish and minor profile changes, worm shafts can be re-ground 1-2 times depending on case depth. Each re-grind removes approximately 0.05-0.10mm. Once the hardened case is ground through, the shaft must be re-hardened or replaced.
What surface finish is achievable on ground hardened steel worm shafts?
Precision thread grinding achieves Ra 0.4 μm routinely. For ultra-high-speed or ultra-quiet applications, additional polishing can achieve Ra 0.2 μm. The surface finish directly impacts friction, efficiency, and noise—smoother finishes extend bronze wheel life significantly.
Related Resources for Hardened Alloy Steel
Worm Gear Grinding
Precision grinding is required after case hardening to achieve DIN 4-5 grade accuracy on worm shafts.
Learn more →AGMA 6022 Standard
AGMA quality grades for hardened steel worm shafts used in automotive and precision industrial applications.
Learn more →Machine Tools
Hardened steel worm shafts with ground threads are the standard for CNC rotary tables and indexing drives.
Learn more →Automotive
Case-hardened steel shafts power EPS systems, seat adjusters, and sunroof mechanisms in vehicles.
Learn more →