Worm Gear Terminology: A–Z Glossary
This glossary defines the worm gear terminology used throughout our design guides, product pages, and engineering drawings — 40+ entries written for mechanical and procurement engineers, technical translators, and anyone new to worm gearing. Terms are grouped into four areas: geometry (module, lead angle, pressure angle), manufacturing and heat treatment (hobbing, grinding, carburizing), materials (phosphor bronze, case-hardening steels, engineering plastics), and standards (AGMA 6022, DIN 3974, ISO 54, JIS B 1723). Each entry gives a short definition, related gear terminology, and a link to a deeper resource. Use the category filter above or jump straight to a letter below.
1
16MnCr5
MaterialsA European case-hardening steel standard for worm shafts.
16MnCr5 (DIN standard) is a low-carbon chromium-manganese steel designed for case hardening. After carburizing and quenching, it achieves a hard surface (58-64 HRC) with a tough core (28-32 HRC). It offers excellent hardenability, good machinability before heat treatment, and minimal distortion. It is the European equivalent of AISI 8620 and is widely used for precision worm shafts in industrial gearboxes.
8
8620
MaterialsAn American nickel-chromium-molybdenum case-hardening steel for worm shafts.
AISI 8620 is a low-carbon Ni-Cr-Mo steel widely used for carburized worm shafts in North America. It provides excellent fatigue resistance, toughness, and wear resistance after case hardening. Core hardness of 28-32 HRC and case hardness of 58-64 HRC are typical. Its nickel content provides superior toughness compared to plain chromium steels. It is the American equivalent of European 16MnCr5 and Japanese SCM420.
A
Aluminum Bronze
(CuAl10Fe3)MaterialsA high-strength copper-aluminum alloy with superior corrosion resistance for heavy-duty applications.
Aluminum bronze (CuAl10Fe3, C63000) offers higher strength and better corrosion resistance than phosphor bronze. It is preferred for marine, offshore, mining, and heavy-load industrial drives. The aluminum content forms a hard aluminum oxide surface layer that resists wear and cavitation erosion. It handles shock loads better than phosphor bronze and maintains properties at elevated temperatures. Hardness ranges from 150-220 HB.
See the aluminum bronze material page for heavy-duty worm wheel options.
AGMA 6022
StandardsThe American Gear Manufacturers Association standard for cylindrical wormgear design and rating.
AGMA 6022 is the American Gear Manufacturers Association design manual for cylindrical wormgearing (current edition: ANSI/AGMA 6022-D19, reaffirmed 2025). It provides formulas and guidance for load capacity (pitting resistance, bending strength, scoring resistance), thermal rating, efficiency estimation, and lubrication selection. AGMA 6022 is a design and rating document, not an accuracy/tolerance standard. Wormgear tolerances and inspection methods are covered by ANSI/AGMA 2011-B14; the legacy Q3–Q15 quality numbers for parallel-axis gears were defined in AGMA 2000-A88 and replaced by ANSI/AGMA 2015-1-A01 (grades A2–A11). For procurement, specify an accuracy standard for tooth tolerances and AGMA 6022 for load-capacity verification.
See the AGMA 6022 reference page for design and rating requirements.
B
Backlash
BasicsThe angular clearance between mating gear teeth necessary for lubrication and thermal expansion.
Backlash is the amount of rotation the worm wheel can move without engaging the worm. It is necessary to accommodate manufacturing tolerances, thermal expansion, and lubricant film thickness. However, excessive backlash reduces positioning accuracy. Backlash is controlled by adjusting wheel thickness, center distance, or using specialized designs such as split wheels or dual-worm systems. Typical backlash ranges from 0.02mm (precision) to 0.30mm (general industrial).
Backlash is set and verified during assembly — see the installation guide for adjustment procedures.
Backdriving
BasicsReverse power flow from the wheel to the worm, possible when the gear set is not self-locking.
Backdriving occurs when torque applied at the worm wheel rotates the worm in reverse. It happens when the lead angle exceeds the friction angle — the condition opposite to self-locking. Multi-start worms with lead angles above roughly 10–15° backdrive readily. This is desirable in servo axes, where energy must flow in both directions, but lifting and hoisting applications need a brake or holding motor to prevent unintended reverse motion when power is removed.
C
Center Distance
GeometryThe distance between the axes of the worm and worm wheel.
Center distance (a) is the fundamental mounting dimension for a worm gear set. It is calculated as a = (d1 + d2) / 2, where d1 is the worm pitch diameter and d2 is the wheel pitch diameter. Standard center distances follow preferred number series: 40, 50, 63, 80, 100, 125, 160, 200, 250, 315, 400, 500 mm. Adjustable center distance is used to control backlash during assembly.
Contact Pattern
ManufacturingThe area of tooth contact visible when marking compound is applied between mating gears.
Contact pattern reveals how load is distributed across the tooth face. An ideal pattern is centered on the tooth face, covering 60-80% of the face width without reaching the edges or tips. Edge contact indicates misalignment or deflection. Tip contact indicates incorrect center distance. Contact pattern is verified during assembly by applying marking compound, rotating the worm, and inspecting the pattern on the wheel teeth. Matched worm gear sets are factory-adjusted for optimal contact pattern.
Contact pattern inspection is part of correct commissioning — see the installation guide.
Carburizing
Heat TreatmentA heat treatment process that diffuses carbon into the surface of low-carbon steel to create a hard case.
Carburizing is the most common heat treatment for worm shafts. The steel part is heated in a carbon-rich atmosphere (gas, liquid, or solid) at 850-950 degrees C, causing carbon to diffuse into the surface layer. After quenching and tempering, the surface reaches 58-64 HRC while the core remains tough at 28-32 HRC. Effective case depth ranges from 0.5mm to 1.5mm depending on application requirements. Carburizing provides excellent wear resistance and fatigue strength.
D
Diametral Pitch
(DP)GeometryThe imperial equivalent of module, equal to number of teeth divided by pitch diameter in inches.
Diametral Pitch (DP) = z / d (inches), the inverse of module. Common DP values include 32, 24, 16, 12, 10, 8, 6, 5, 4. Higher DP means smaller teeth. To convert: m = 25.4 / DP. Diametral pitch is used primarily in North American markets, while module is standard in Europe and Asia.
See Module for the metric equivalent and standard series.
DIN 3974
StandardsThe German standard defining tolerances for cylindrical worm gears.
DIN 3974 specifies accuracy grades from 1 (highest) to 12 (lowest) for cylindrical worm gears. Grades 3-6 represent precision ground gears, 7-9 hobbed or milled gears, and 10-12 rough or cast gears. It controls single pitch deviation, cumulative pitch deviation, profile form deviation, and helix deviation. For DIN 5 grade with module 2.0, single pitch deviation must not exceed 0.005mm. DIN 3974 is the dominant standard in Europe and is widely referenced globally.
See the DIN 3974 reference page for tolerance tables by accuracy grade.
DIN 780
StandardsThe German standard defining preferred module series for gears.
DIN 780 specifies the standard module series used for metric gears: 0.5, 0.6, 0.8, 1.0, 1.25, 1.5, 2.0, 2.5, 3.0, 4.0, 5.0, 6.0, 8.0, 10.0, 12.0, 16.0, 20.0. Using standard modules ensures that cutting tools, measuring instruments, and mating gears are readily available. Custom modules are possible but require custom tooling, increasing cost and lead time. DIN 780-2 is the part dedicated to cylindrical worm gear transmissions; DIN 780 modules are equivalent to ISO 54 modules.
Double-Enveloping Worm Gear
GeometryA worm gear set in which both the worm and the wheel are throated to partially wrap around each other.
In a double-enveloping (globoid or hourglass) worm gear set, the worm is machined with a concave body that wraps around the wheel, and the wheel face is throated to match the worm. Both members conform to each other's curvature, putting significantly more teeth in simultaneous contact than a cylindrical (single-enveloping) set. This distributes load over a larger contact area, increasing torque capacity and stiffness in the same envelope. Double-enveloping sets must be manufactured as matched pairs and are not interchangeable.
Duplex Worm
GeometryA worm with different leads on the two thread flanks, allowing backlash adjustment by axial shift.
A duplex (dual-lead) worm has a different lead — and therefore a different lead angle — on each flank of the same thread, so the thread thickness varies continuously along the axis. Axially shifting the worm changes the effective tooth thickness in mesh, which adjusts backlash without changing the center distance. Backlash can be set near zero and re-adjusted as the set wears, making duplex worms common in rotary tables, indexing drives, and robotics.
E
Efficiency
BasicsThe ratio of output power to input power, typically 50-90% for worm gears depending on design.
Worm gear efficiency is primarily determined by lead angle: smaller angles (single-start worms) yield 50-70% efficiency, while larger angles (multi-start worms) reach 80-90%. Lost energy converts to heat due to sliding friction. Efficiency is also affected by speed, lubrication quality, surface finish, and material pairing. For continuous-duty applications, heat generated by inefficiency must be managed through housing design, cooling fins, or forced ventilation.
F
Face Width
GeometryThe axial length of the worm thread or the radial width of the worm wheel teeth.
For worm shafts, face width is the length of the threaded portion. For worm wheels, face width is the width of the tooth rim in the axial direction. Face width affects load capacity: wider teeth distribute load over more surface area. However, excessive face width can cause edge loading if the worm deflects. Typical face width is 0.6 to 1.0 times the worm outer diameter.
G
Grinding
ManufacturingA precision finishing process using abrasive wheels to achieve tight tolerances on hardened gears.
Grinding is used for worm shafts requiring DIN 4-5 grade precision. Continuous generating grinding uses a dressed grinding wheel that follows a generating path to create the involute thread profile. Profile grinding uses a form-dressed wheel matching the exact thread profile. Grinding achieves profile deviations under 0.005mm, pitch error under 0.003mm, and surface finish Ra 0.4 um. It is performed after heat treatment on hardened steel (58-64 HRC).
Our CNC worm grinding process holds DIN 4–5 grade on hardened worms.
Gray Cast Iron
(EN-GJL-250)MaterialsAn economical iron-carbon alloy with excellent damping properties for low-speed worm wheels.
Gray cast iron (GG25, ASTM A48 Class 30) is the most economical worm wheel material. Its graphite flakes provide excellent vibration damping, reducing noise in low-speed applications. However, it has lower wear resistance than bronze, higher friction, and poor shock resistance. It is suitable for manual valve operators, light conveyor drives, and agricultural machinery where cost is the primary concern. Hardness ranges from 180-260 HB.
H
Hobbing
ManufacturingA gear manufacturing process using a rotating cutting tool (hob) to generate gear teeth.
Hobbing is the most common method for manufacturing worm wheels. A hob with the inverse profile of the desired tooth form rotates while the workpiece turns in synchronized motion. The hob feeds radially into the blank to full tooth depth. For worm wheels, the hob must match the mating worm's thread profile to ensure correct meshing. Hobbing achieves DIN 6-8 grade accuracy and is faster and more economical than grinding for standard precision.
See our worm gear hobbing process for achievable accuracy grades and lead times.
I
Induction Hardening
Heat TreatmentA localized heat treatment using electromagnetic induction to rapidly heat and quench specific areas.
Induction hardening uses high-frequency alternating current to heat the surface layer of a steel part in seconds, followed by immediate water or polymer quenching. It produces a hard surface (55-63 HRC) with a sharp transition to the unhardened core. It is faster than carburizing and produces less overall distortion because only the surface is heated. It is suitable for large worms where furnace carburizing would be impractical, but the hardened depth is shallower and less uniform than carburizing.
ISO 54
StandardsThe international standard for preferred module series, equivalent to DIN 780.
ISO 54 defines the same module series as DIN 780: 0.5, 0.6, 0.8, 1.0, 1.25, 1.5, 2.0, 2.5, 3.0, 4.0, 5.0, 6.0, 8.0, 10.0, 12.0, 16.0, 20.0. It is the international equivalent of DIN 780 and is referenced in global gear specifications. Using ISO standard modules ensures interchangeability and availability of cutting tools worldwide.
J
JIS B 1723
StandardsThe Japanese Industrial Standard for cylindrical worm gear tooth profiles and accuracy.
JIS B 1723:2014, Dimensions of Cylindrical Worm Gears, is the Japanese Industrial Standard for general-purpose cylindrical worm gears with axial module 1–25 mm and center distance 40–500 mm. It specifies worm and wheel dimensions, tooth profiles, and accuracy grades 0 (highest) through 8 (lowest). Grades 0-2 represent ultra-precision ground gears, 3-5 precision gears, and 6-8 general industrial gears. Japanese machine tool and robotics manufacturers typically require JIS grade 3 or better. The standard places particular emphasis on thread lead accuracy and profile consistency. JIS grade 3 approximately corresponds to DIN 5 and AGMA Q12-Q13.
See the JIS B 1723 reference page for dimensional requirements.
L
Lead Angle
GeometryThe angle between the worm thread and a plane perpendicular to the worm axis.
Lead angle (gamma) is calculated as tan(gamma) = (m * z1) / d1, where m is module, z1 is number of starts, and d1 is worm pitch diameter. A smaller lead angle increases self-locking tendency but reduces efficiency. Single-start worms typically have lead angles of 3-8 degrees. Multi-start worms reach 15-30 degrees. Lead angle is the primary factor determining worm gear efficiency and self-locking behavior.
Lead angle is the main driver of worm gear efficiency — see how it affects losses and heat.
Lapping
ManufacturingA finishing process using abrasive compound to improve surface finish and optimize contact between mating gears.
Lapping improves the surface finish and contact pattern of bronze worm wheels. A fine abrasive compound is applied between the worm and wheel while they rotate under light load. The abrasive removes high spots and improves conformity between the mating surfaces. Lapping can reduce surface roughness by 30-50% and improve the contact pattern. It is often performed as a final step after hobbing, especially for precision applications.
Lead & Axial Pitch
GeometryThe axial distance between adjacent worm threads (pitch) and the axial advance per revolution (lead).
Axial pitch (px) is the distance between corresponding points on adjacent worm threads, measured parallel to the axis: px = π × m. Lead (L) is the axial distance the thread advances in one full revolution: L = px × z1, where z1 is the number of starts. On a single-start worm, lead equals pitch; on a double-start worm, the lead is twice the pitch. Confusing the two is a common drawing error — a 2-start, module 2 worm has a pitch of 6.28 mm but a lead of 12.57 mm.
M
Module
(m)GeometryA standardized measure of gear tooth size, equal to pitch diameter divided by number of teeth.
Module (m) is the fundamental parameter defining gear tooth size in the metric system. It is calculated as m = d / z, where d is the pitch diameter and z is the tooth count. Standard modules follow DIN 780 or ISO 54 series: 0.5, 0.6, 0.8, 1.0, 1.25, 1.5, 2.0, 2.5, 3.0, 4.0, 5.0, 6.0, 8.0, 10.0, 12.0, 16.0, 20.0. Larger modules produce stronger teeth but increase gear size. The module must be identical for the worm and wheel in a given set.
Use the worm gear design guide to choose module, center distance, and ratio for your application.
Multi-Start Worm
GeometryA worm with two or more parallel threads wrapping around the shaft.
Multi-start worms have 2, 3, or 4 parallel threads. They provide higher efficiency (up to 90%) and faster output speed than single-start worms but sacrifice transmission ratio and self-locking. A double-start worm with a 40-tooth wheel gives a 20:1 ratio. Multi-start worms are used in power transmission applications where efficiency is more important than holding torque.
Compare the trade-offs in multi-start vs single-start worm gears.
N
Nitriding
Heat TreatmentA heat treatment that diffuses nitrogen into steel surface to create a very hard, thin case with minimal distortion.
Nitriding diffuses nitrogen into the steel surface at 500-550 degrees C (below the transformation temperature), producing a hard case with minimal dimensional change. Surface hardness reaches 65-72 HRC with case depths of 0.1-0.5mm. Because nitriding occurs at lower temperatures than carburizing, distortion is minimal, making it ideal for large, precision-ground worms where post-heat-treatment grinding would be expensive. It requires steel with nitride-forming elements (Cr, Mo, Al) such as 42CrMo4 or 4140.
P
Pressure Angle
GeometryThe angle between the line of action and the tangent to the pitch circle at the pitch point.
Standard pressure angle for worm gears is 20 degrees, though 14.5 degrees and 25 degrees are also used. The pressure angle affects tooth strength, contact ratio, and undercutting tendency. Higher pressure angles produce stronger teeth but increase separation force and bearing load. Worm gear pressure angle is defined in the normal plane to the worm thread.
Pitch Diameter
GeometryThe diameter of the imaginary cylinder where the worm and wheel theoretically mesh.
For the worm, pitch diameter (d1) = m * q, where q is the worm diameter factor (typically 8-16). For the wheel, pitch diameter (d2) = m * z2. The pitch diameter is not the same as the outer diameter or root diameter. All gear calculations (ratio, center distance, lead angle) are based on pitch diameter.
Profile Deviation
ManufacturingThe difference between the actual tooth profile and the theoretical ideal profile.
Profile deviation measures how closely the manufactured tooth shape matches the designed involute or convolute profile. It is measured using a CMM or gear measurement center. For DIN 5 grade, total profile deviation (Fa) must be under 0.006mm for module 2.0. Excessive profile deviation causes uneven load distribution, noise, and premature wear. Profile deviation is controlled by tool accuracy, machine setup, and thermal stability during machining.
Phosphor Bronze
(CuSn8P)MaterialsA copper-tin alloy with phosphorus addition, the standard material for worm wheels.
Phosphor bronze (CuSn8P to CuSn12P) is the most common worm wheel material. Tin content (8-12%) provides hardness and wear resistance, while phosphorus improves casting fluidity and machinability. It exhibits a low coefficient of friction against steel (0.03-0.08 under lubrication) and excellent resistance to scoring and galling. Hardness ranges from 80-180 HB depending on composition and heat treatment. It is the standard choice for general industrial, elevator, automotive, and valve actuator applications.
See the phosphor bronze material page for grades, hardness, and casting methods.
POM
(Polyacetal)MaterialsAn engineering plastic used for low-noise, lubrication-free miniature worm gears.
POM (polyacetal, Delrin) is the most widely used plastic for miniature worm wheels. It offers excellent dimensional stability, low friction coefficient (0.15-0.35 against steel), and good fatigue resistance. POM gears run 10-20 dB quieter than metal gears and often operate without lubrication. FDA-compliant grades are available for medical and food-contact applications. Operating temperature limit is approximately 100 degrees C.
See engineering plastic worm gear materials for POM, PA66, and PEEK options.
PEEK
(Polyether Ether Ketone)MaterialsA high-performance thermoplastic with exceptional temperature and chemical resistance.
PEEK is used for worm gears in extreme environments: continuous operation up to 250 degrees C, aggressive chemicals, and radiation exposure. It is non-magnetic (MRI-compatible) and can withstand autoclave sterilization cycles. PEEK gears are significantly more expensive than POM but offer unmatched performance in demanding medical, aerospace, and chemical processing applications. It can be reinforced with carbon fiber or glass fiber for higher strength.
See our engineering plastic materials page for PEEK worm gear capabilities.
Pitting
Failure AnalysisSurface fatigue damage appearing as small craters on gear teeth caused by repeated contact stress.
Pitting occurs when contact stress exceeds the material's endurance limit over many cycles. In worm gears, it typically begins on bronze wheels because bronze has lower fatigue strength than hardened steel. Subsurface cracks initiate at stress concentrations and propagate to the surface, detaching small material particles. Prevention includes reducing contact stress, using higher-strength bronze alloys, ensuring adequate lubricant film thickness, and proper run-in during initial operation.
Q
Quenching and Tempering
Heat TreatmentA heat treatment process of heating steel above its critical temperature, rapid cooling, then reheating to improve toughness.
Quenching and tempering (Q+T) is used for through-hardened steels where uniform hardness is desired throughout the cross-section. The steel is heated to 820-880 degrees C, quenched in oil or water, then tempered at 150-650 degrees C to achieve the desired hardness-toughness balance. For worm shafts, Q+T is less common than case hardening because a hard surface on a tough core provides better wear resistance and fatigue performance.
R
Run-In
ManufacturingInitial operation of a new gear set under gradually increasing load to polish surfaces and verify performance.
Run-in involves operating a new worm gear set at 25% rated load for 2-4 hours, then 50% load for 4-8 hours, before full-load operation. This process work-hardens the bronze wheel surface, polishes minor machining irregularities, establishes a compatible oil film, and verifies that temperature and noise are within specifications. Run-in is essential for maximizing service life and is standard practice for all precision worm gear sets.
Follow the staged run-in schedule in our installation guide before applying full load.
S
Self-Locking
BasicsThe property of a worm gear set that prevents the wheel from driving the worm backwards.
Self-locking occurs when the lead angle of the worm is smaller than the friction angle between the worm and wheel materials. In this condition, the friction force is sufficient to prevent back-driving. Single-start worms with small lead angles (typically under 5-6 degrees) usually exhibit self-locking. This property is valuable for safety-critical applications such as elevators, hoists, and jacks where the load must remain stationary when power is removed. Multi-start worms with larger lead angles are generally reversible.
See our self-locking worm gear product line for safety-critical holding applications.
Single-Start Worm
GeometryA worm with one continuous thread wrapping around the shaft.
A single-start worm (z1=1) provides the highest transmission ratio per wheel revolution. For a 40-tooth wheel, the ratio is 40:1. Single-start worms have small lead angles (3-8 degrees) and typically exhibit self-locking. They are used in lifting, positioning, and safety-critical applications. Efficiency is lower (50-70%) compared to multi-start worms.
Surface Finish
ManufacturingThe microscopic texture of a machined surface, typically measured as Ra (arithmetic average roughness).
Surface finish is critical for worm gears because it affects friction, efficiency, and lubricant film formation. Ground precision worms achieve Ra 0.2-0.4 um. Hobbed worms achieve Ra 0.8-1.6 um. Bronze wheels after hobbing achieve Ra 1.6-3.2 um. Smoother surfaces reduce friction losses, improve efficiency, and extend life. Superfinishing or polishing can achieve Ra 0.1 um for the most demanding applications.
SCM420
MaterialsA Japanese chromium-molybdenum case-hardening steel for precision worm shafts.
SCM420 (JIS standard) is a Cr-Mo case-hardening steel equivalent to AISI 8620 and DIN 16MnCr5. It is widely used in Japanese and Asian manufacturing for automotive and industrial worm shafts. After carburizing and quenching, it achieves 58-64 HRC surface hardness with excellent fatigue resistance. It offers good machinability in the annealed condition and responds well to heat treatment.
Stress Relieving
Heat TreatmentA low-temperature heat treatment to reduce internal stresses without significantly changing mechanical properties.
Stress relieving heats the part to 550-650 degrees C (below the transformation temperature), holds for 1-2 hours, then cools slowly. It reduces internal stresses from machining, welding, or heat treatment without significantly affecting hardness. For worm shafts, stress relieving after rough machining and before finish grinding prevents distortion during final machining. It is also performed after welding operations on large worm assemblies.
Scoring
Failure AnalysisAdhesive wear caused by metal-to-metal contact when the lubricant film breaks down.
Scoring (also called scuffing) occurs when sliding contact causes localized welding and tearing between the worm and wheel. It appears as scratches, grooves, or smeared material parallel to the sliding direction. It is accelerated by high sliding speeds, inadequate lubrication, excessive load, or high temperatures that degrade oil viscosity. Prevention requires maintaining robust elastohydrodynamic lubrication through proper oil viscosity, EP additives, and temperature control.
T
Transmission Ratio
BasicsThe ratio of output speed to input speed, equal to wheel tooth count divided by worm starts.
Transmission ratio (i) = z2 / z1, where z2 is the number of teeth on the worm wheel and z1 is the number of starts on the worm. For a single-start worm (z1=1) with a 40-tooth wheel (z2=40), the ratio is 40:1. Higher ratios provide greater torque multiplication but reduce efficiency and output speed. Single-stage worm gears typically achieve ratios from 5:1 to 100:1.
Throated Wheel
GeometryA worm wheel with a concave face that matches the curvature of a double-enveloping worm.
In double-enveloping (hourglass) worm gear sets, the wheel has a concave (throated) face that conforms to the curved profile of the worm. This geometry increases the number of teeth in simultaneous contact, distributing load and increasing torque capacity. Throated wheels are more expensive to manufacture than flat-faced wheels and must be produced as matched pairs with their worms.
U
Undercutting
GeometryRemoval of tooth material at the base due to tool interference during manufacturing.
Undercutting occurs when the cutting tool removes material below the involute profile at the tooth root, weakening the tooth. It is caused by low tooth counts or incorrect tool geometry. In worm gears, undercutting of the wheel is avoided by using sufficient tooth count (typically z2 >= 20) and proper hob design. Undercutting reduces bending strength and can cause stress concentration.
W
Worm
BasicsA screw-like shaft that meshes with a worm wheel to transmit motion and power between perpendicular shafts.
The worm is the driving member of a worm gear set. It resembles a screw with a trapezoidal or involute thread profile. As the worm rotates, its threads engage with the helical teeth of the worm wheel. Key geometric parameters include the lead angle, module, number of starts, and thread profile type (ZA, ZI, ZK, ZN). Worms are typically manufactured from hardened alloy steel (16MnCr5, 8620, SCM420) and are the high-speed input member of the gear set.
Worm Wheel
BasicsA helical gear that meshes with a worm shaft, typically the driven member of a worm gear set.
The worm wheel (also called worm gear) is the driven member that receives motion from the worm. It has helical teeth shaped to match the worm thread profile. Worm wheels are commonly made from bronze (phosphor bronze or aluminum bronze) for low friction and wear resistance, cast iron for low-cost applications, or engineering plastics for miniature gears. The wheel's tooth count determines the transmission ratio when divided by the worm's number of starts.
Worm Diameter Factor
(q)GeometryThe ratio of worm pitch diameter to module: q = d1 / m.
The worm diameter factor (q) typically ranges from 8 to 16. Higher q values produce larger, stiffer worms with better load distribution but require larger center distances. Lower q values (8-10) produce compact designs but may suffer from shaft deflection. Precision applications typically use q >= 10 to minimize deflection under load.
Frequently Asked Questions About Worm Gear Terminology
What is the difference between module and diametral pitch?
Module (m) and diametral pitch (DP) describe the same thing — tooth size — in different unit systems. Module is metric: m = pitch diameter ÷ tooth count, in millimeters. Diametral pitch is imperial: DP = tooth count ÷ pitch diameter in inches. They convert exactly: m = 25.4 ÷ DP. A DP 12 gear equals module 2.117; a module 2 gear equals DP 12.7. The worm and wheel in a set must always share the same module or DP.
What is the difference between lead and pitch on a worm?
Axial pitch is the distance between adjacent threads measured parallel to the worm axis; lead is how far the thread advances in one full revolution. Lead = axial pitch × number of starts. A single-start worm's lead equals its pitch, but a three-start worm advances three pitches per turn. Lead — not pitch — sets the lead angle, which controls efficiency and self-locking.
How much backlash is normal in a worm gear set?
Typical backlash ranges from about 0.02 mm for precision ground sets to 0.30 mm for general industrial drives. Some clearance is necessary for lubrication and thermal expansion; too little causes binding and overheating, while too much hurts positioning accuracy. Backlash is adjusted through center distance, wheel thickness, split wheels, or duplex (dual-lead) worms, and it should be re-checked after run-in.
Is AGMA 6022 the same standard as DIN 3974?
No — they do different jobs and are often used together. AGMA 6022 (current edition ANSI/AGMA 6022-D19) is an American design manual covering load capacity, thermal rating, and efficiency of cylindrical wormgearing. DIN 3974 (parts 1 and 2, 1995) is a German accuracy standard defining tolerance grades 1–12 for worm and wheel tooth geometry. Specify DIN 3974 for manufacturing tolerances, and use AGMA 6022 to verify the design's load rating.
Why are single-start worm gears self-locking?
Self-locking occurs when the worm's lead angle is smaller than the friction angle between the worm and wheel. Friction then exceeds the back-driving component of the load, so the wheel cannot turn the worm. Single-start worms have small lead angles — typically 3–8° — and usually self-lock below about 5–6°. This makes them ideal for hoists and jacks, but note that vibration or worn surfaces can reduce the locking margin.
What accuracy grade should I specify for a precision worm gear?
For precision applications such as servo drives, indexing tables, and robotics, specify DIN 3974 grade 4–5, which requires ground worms after heat treatment. General industrial drives run well at grades 7–9 with hobbed teeth; grades 10–12 suit rough, low-speed mechanisms. As a rough cross-reference, DIN 5 corresponds approximately to JIS grade 3. State the standard, grade, and module on the drawing — "ground to DIN 5" is enough for most suppliers to quote.